MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Vitiva PC715 PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damaging wavelengths of light, protecting the contents of the package. In addition, Vitiva PET allows brand owners to achieve uniquely shaped containers with extraordinary clarity thereby showcasing the contents of the package.

Applications/Uses

  • Cosmetics
  • Health and nutrition containers
  • Household products containers
  • Pharmaceutical containers
  • Custom bottles
  • Hotfilled food and beverage containers
  • Personal care
  • Key Attributes

  • Chemical compatibility with packaged goods
  • Drop-in replacement for standard PET
  • Exceptional drop impact strength
  • Meets FDA regulations for food contact
  • Unlimited recyclability
  • Excellent clarity
  • Excellent oxygen gas barrier
  • FDA-compliant UV light barrier
  • Virtually unlimited bottle design freedom
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Bulk Density 0.818 g/ccPoured; ASTM D1895
     0.888 g/ccVibrated; ASTM D1895
    Density 1.40 g/ccCrystalline Density; ASTM D1505
    Melt Density 1.20 g/cc
    @Temperature 285 °C
    ASTM D1238
    Particle Size 2500 µmPellet Size
    Viscosity Measurement 0.76 - 0.80Intrinsic; VGAS-A-AN-G-V-1
     
    Thermal PropertiesOriginal ValueComments
    Heat of Fusion 63.0 J/gASTM E793
    Specific Heat Capacity 1.20 J/g-°CASTM E1269
     1.40 J/g-°C
    @Temperature 80.0 °C
    ASTM E1269
     1.50 J/g-°C
    @Temperature 100 °C
    ASTM E1269
     1.80 J/g-°C
    @Temperature 200 °C
    ASTM E1269
     2.00 J/g-°C
    @Temperature 280 °C
    ASTM E1269
    Melting Point 247 °CCrystalline Peak; ASTM D3418
     
    Optical PropertiesOriginal ValueComments
    UV Transmittance <= 7.0 %
    @Thickness 0.229 mm,
    Wavelength 370 nm
    well-oriented bottle sidewalls; VCSC-A-AS-G-CA-0005
     
    Descriptive Properties
    Acetaldehyde<3ppmVKCA-A-AS-G-GC-0001
    Color, CIE a*-1.5 ± 2.0VGAS-A-AN-G-RS-001
    Color, CIE b*0.5 ± 1.7VGAS-A-AN-G-RS-001
    Color, CIE L*77.8 minVGAS-A-AN-G-RS-001
    Fines, wt%, max0.1
    Pellet ShapeCubical

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
    Wellman PermaClear™ HP806 (0.84 IV) PET
    Overview of materials for Polycarbonate/PET Polyester Blend
    Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)
    CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade

    PE9124 / 35181

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.