Physical Properties | Metric | English | Comments |
---|
Density | 1.12 - 1.47 g/cc | 0.0405 - 0.0531 lb/in³ |
Water Absorption | 0.0500 - 0.900 % | 0.0500 - 0.900 % |
Moisture Absorption at Equilibrium | 0.0200 - 0.700 % | 0.0200 - 0.700 % |
Water Absorption at Saturation | 0.200 - 0.750 % | 0.200 - 0.750 % |
Viscosity | 200 - 600 cP @Temperature 260 - 270 °C | 200 - 600 cP @Temperature 500 - 518 °F |
| 200 - 600 cP @Frequency 165 - 1000 Hz | 200 - 600 cP @Frequency 165 - 1000 Hz |
Maximum Moisture Content | 0.00200 - 0.0200 | 0.00200 - 0.0200 |
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in |
| 0.00800 - 0.00800 cm/cm @Temperature 80.0 - 80.0 °C | 0.00800 - 0.00800 in/in @Temperature 176 - 176 °F |
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in |
| 0.00800 - 0.00800 cm/cm @Temperature 80.0 - 80.0 °C | 0.00800 - 0.00800 in/in @Temperature 176 - 176 °F |
Melt Flow | 3.00 - 43.0 g/10 min | 3.00 - 43.0 g/10 min |
Ash | 10.0 - 20.0 % | 10.0 - 20.0 % |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell R | 108 - 120 | 108 - 120 |
Hardness, Shore D | 73.0 | 73.0 |
Tensile Strength, Ultimate | 36.0 - 108 MPa | 5220 - 15700 psi |
Tensile Strength, Yield | 34.0 - 108 MPa | 4930 - 15700 psi |
Elongation at Break | 2.10 - 200 % | 2.10 - 200 % |
Elongation at Yield | 2.00 - 86.0 % | 2.00 - 86.0 % |
Modulus of Elasticity | 1.16 - 7.65 GPa | 168 - 1110 ksi |
Flexural Yield Strength | 50.0 - 153 MPa | 7250 - 22200 psi |
Flexural Modulus | 1.14 - 7.03 GPa | 165 - 1020 ksi |
Flexural Strain at Yield | 5.00 - 6.20 % | 5.00 - 6.20 % |
Izod Impact | 51.0 - 580 J | 37.6 - 428 ft-lb |
Izod Impact, Notched | 0.392 - 100 J/cm | 0.735 - 187 ft-lb/in |
| 0.0500 - 7.50 J/cm @Temperature -40.0 - -20.0 °C | 0.0937 - 14.1 ft-lb/in @Temperature -40.0 - -4.00 °F |
| 0.490332 - 7.50 J/cm @Temperature -40.0 - -22.0 °C | 0.918594 - 14.1 ft-lb/in @Temperature -40.0 - -7.60 °F |
| 0.490332 - 7.50 J/cm @Thickness 3.17 - 6.35 mm | 0.918594 - 14.1 ft-lb/in @Thickness 0.125 - 0.250 in |
Izod Impact, Unnotched | 5.58 J/cm - NB | 10.5 ft-lb/in - NB |
| NB - NB @Temperature -40.0 - -40.0 °C | NB - NB @Temperature -40.0 - -40.0 °F |
Izod Impact, Notched (ISO) | 1.00 - 75.0 kJ/m² | 0.476 - 35.7 ft-lb/in² |
| 5.00 - 60.0 kJ/m² @Temperature -40.0 - -10.0 °C | 2.38 - 28.6 ft-lb/in² @Temperature -40.0 - 14.0 °F |
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² - NB | 18.1 ft-lb/in² - NB |
| 85.0 kJ/m² - NB @Temperature -30.0 - -30.0 °C | 40.4 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Charpy Impact Unnotched | 5.00 J/cm² - NB | 23.8 ft-lb/in² - NB |
| 8.50 J/cm² - NB @Temperature -30.0 - -30.0 °C | 40.5 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Charpy Impact, Notched | 0.800 - 9.00 J/cm² | 3.81 - 42.8 ft-lb/in² |
| 0.600 - 5.00 J/cm² @Temperature -30.0 - -30.0 °C | 2.86 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Gardner Impact | 36.2 - 36.2 J | 26.7 - 26.7 ft-lb |
Dart Drop, Total Energy | 5.31 - 95.0 J | 3.92 - 70.1 ft-lb |
| 5.13856 - 61.961 J @Temperature -40.0 - 0.000 °C | 3.79000 - 45.700 ft-lb @Temperature -40.0 - 32.0 °F |
| 49.0 - 80.2 J @Temperature -40.0 - 0.000 °C | 36.1 - 59.2 ft-lb @Temperature -40.0 - 32.0 °F |
| 49.0 - 80.2 J @Thickness 3.20 - 3.20 mm | 36.1 - 59.2 ft-lb @Thickness 0.126 - 0.126 in |
Puncture Energy | 36.0 - 55.0 J | 26.6 - 40.6 ft-lb |
| 47.0 - 49.0 J @Temperature -40.0 - -30.0 °C | 34.7 - 36.1 ft-lb @Temperature -40.0 - -22.0 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 8.00e+9 - 1.00e+18 ohm-cm | 8.00e+9 - 1.00e+18 ohm-cm |
Surface Resistance | 9.00e+9 - 1.00e+17 ohm | 9.00e+9 - 1.00e+17 ohm |
Static Decay | 2.00 sec | 2.00 sec |
Dielectric Constant | 3.00 - 4.40 | 3.00 - 4.40 |
Dielectric Strength | 17.0 - 34.0 kV/mm | 432 - 864 kV/in |
Dissipation Factor | 0.00200 - 0.144 | 0.00200 - 0.144 |
Arc Resistance | 60.0 - 121 sec | 60.0 - 121 sec |
Comparative Tracking Index | 100 - 600 V | 100 - 600 V |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 26.0 - 167 µm/m-°C | 14.4 - 93.0 µin/in-°F |
CTE, linear, Transverse to Flow | 45.0 - 140 µm/m-°C | 25.0 - 77.8 µin/in-°F |
Thermal Conductivity | 0.162 - 2.00 W/m-K | 1.12 - 13.9 BTU-in/hr-ft²-°F |
Melting Point | 220 - 280 °C | 428 - 536 °F |
Maximum Service Temperature, Air | 120 °C | 248 °F |
Hot Ball Pressure Test | 85.0 °C | 185 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 79.0 - 255 °C | 174 - 491 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 - 222 °C | 105 - 432 °F |
Vicat Softening Point | 90.0 - 204 °C | 194 - 399 °F |
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F |
Glass Transition Temp, Tg | 92.0 - 150 °C | 198 - 302 °F |
UL RTI, Electrical | 75.0 - 120 °C | 167 - 248 °F |
UL RTI, Mechanical with Impact | 75.0 - 120 °C | 167 - 248 °F |
UL RTI, Mechanical without Impact | 75.0 - 120 °C | 167 - 248 °F |
Flammability, UL94 | HB - 5VA | HB - 5VA |
Glow Wire Test | 750 - 960 °C | 1380 - 1760 °F |
|
Optical Properties | Metric | English | Comments |
---|
Refractive Index | 1.54 - 1.58 | 1.54 - 1.58 |
Haze | 0.300 - 25.0 % | 0.300 - 25.0 % |
Transmission, Visible | 35.0 - 88.0 % | 35.0 - 88.0 % |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 50.0 - 282 °C | 122 - 540 °F |
Nozzle Temperature | 230 - 302 °C | 446 - 575 °F |
Melt Temperature | 210 - 330 °C | 410 - 626 °F |
Head Temperature | 240 - 270 °C | 464 - 518 °F |
Mold Temperature | 18.0 - 110 °C | 64.4 - 230 °F |
Injection Velocity | 200 mm/sec | 7.87 in/sec |
Drying Temperature | 65.0 - 127 °C | 149 - 261 °F |
Moisture Content | 0.0100 - 0.0200 % | 0.0100 - 0.0200 % |
Dew Point | -17.8 °C | 0.000 °F |
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) |
Injection Pressure | 4.96 - 172 MPa | 720 - 25000 psi |
Vent Depth | 0.00130 - 0.0203 cm | 0.000512 - 0.00800 in |
Cushion | 0.635 cm | 0.250 in |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.