MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LE Phenolic Laminate
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Linen based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many structural applications.

Information provided by Aurora Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0500 lb/in³
Water Absorption 1.0 %1.0 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 105105
Tensile Strength, Ultimate 103 MPa15000 psi
Flexural Strength 172 MPa25000 psi
Compressive Strength 262 MPa38000 psi
Shear Strength 96.5 MPa14000 psi
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+10 ohm-cm7.00e+10 ohm-cm
Surface Resistance 6.00e+10 ohm6.00e+10 ohm
Dielectric Constant 5.3
@Frequency 1e+6 Hz
5.3
@Frequency 1e+6 Hz
Dielectric Strength 13.8 kV/mm350 kV/in
Dielectric Breakdown 70000 V70000 V
Dissipation Factor 0.060
@Frequency 1e+6 Hz
0.060
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 115 °C239 °FElectrical
 125 °C257 °FMechanical
 
Descriptive Properties
ColorNatural/Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-3 Fiberglass Phenolic Laminate Sheet
G-10 Fiberglass Epoxy Laminate Sheet
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
CE Phenolic Laminate
Norplex-Micarta NP193PM Phenolic Laminate Sheet

PGLAM21 / 41892

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.