MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CE Phenolic Laminate
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many structural applications.

Information provided by Aurora Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0500 lb/in³
Water Absorption 1.1 %1.1 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 105105
Tensile Strength, Ultimate 89.6 MPa13000 psi
Flexural Strength 131 MPa19000 psi
Compressive Strength 255 MPa37000 psi
Shear Strength 68.9 MPa10000 psi
Izod Impact, Notched 0.961 J/cm1.80 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 7.87 kV/mm200 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 115 °C239 °FElectrical
 125 °C257 °FMechanical
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-3 Fiberglass Phenolic Laminate Sheet
LE Phenolic Laminate
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Ensinger Tecapeek® Polyetheretherketone (PEEK)
XXX Phenolic Laminate

PGLAM20 / 41891

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.