MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Proto3000 ABSi Fused Deposition Modeling Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Description: Stratasys ABSi is an ideal material for conceptual modeling, functional prototyping and direct digital manufacturing. Its strength is superior to standard Stratasys ABS, and the translucent nature of ABSi beneficial for monitoring material flow and light transmission, most commonly used for medical and automotive applications. ABSi gives you Real Parts™ that are visually unique, dimensionally accurate, durable and hold their shape over time

Available Colors: Translucent Natural, Translucent Amber and Translucent Red

Information provided by Proto3000 for their protoyping engineering services.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength at Break 37.0 MPa5370 psiType 1, 2"/min; ASTM D638
Elongation at Break 4.4 %4.4 %ASTM D638
Tensile Modulus 1.915 GPa277.7 ksiASTM D638
Flexural Strength 62.0 MPa8990 psiMethod 1, 0.05"/min; ASTM D790
Flexural Modulus 1.917 GPa278.0 ksiASTM D790
Izod Impact, Notched 0.964 J/cm1.81 ft-lb/inMethod A; ASTM D256
Izod Impact, Unnotched 1.911 J/cm3.580 ft-lb/inMethod A; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 121 µm/m-°C67.2 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
@Thickness 0.125 mm
187 °F
@Thickness 0.00492 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
@Thickness 0.125 mm
163 °F
@Thickness 0.00492 in
unannealed; ASTM D648
Glass Transition Temp, Tg 116 °C241 °FDAM (SSYS)
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Stratasys® ABSi
Stratasys® PC-ABS
Stratasys® Ultem 9085 for Rapid Prototyping
Clariant Acrylonitrile Butadiene Styrene, White 3D Printer Filament

PPROTO968 / 133171

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.