MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Viton® B-303C Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • high quality, smooth extrudate surface and appearance at thickness below .040” or 1.0mm
  • excellent ‘green’ strength that helps maintain extrudate shape as well as enabling draw down to very thin veneer thicknesses
  • excellent fuel permeation resistance
  • good tensile strength
  • good adhesion to other elastomers in multilayer hoses

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.875 g/cc1.875 g/ccUncompounded Viton
Mooney Viscosity 30
@Temperature 121 °C
30
@Temperature 250 °F
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7474No Postcure; ASTM D2240
 767616 hours Postcure at 232 degrees C; ASTM D2240
Tensile Strength at Break 7.90 MPa1150 psiASTM D412
 11.0 MPa1600 psiASTM D412
Tensile Stress at Strain  1.20 MPa
@Strain 10 %
174 psi
@Strain 10 %
No Postcure; ASTM D412
 1.50 MPa
@Strain 10 %
218 psi
@Strain 10 %
16 hours Postcure at 232 degrees C; ASTM D412
 1.90 MPa
@Strain 25 %
276 psi
@Strain 25 %
No Postcure; ASTM D412
Elongation at Break 260 %260 %16 hours Postcure at 232 degrees C; ASTM D412
 359 %359 %No Postcure; ASTM D412
100% Modulus  3.50 MPa
@Strain 100 %
508 psi
@Strain 100 %
No Postcure; ASTM D412
 4.70 MPa
@Strain 100 %
682 psi
@Strain 100 %
16 hours Postcure at 232 degrees C; ASTM D412
Compression Set  25 %
@Temperature 150 °C,
Time 252000 sec
25 %
@Temperature 302 °F,
Time 70.0 hour
Plied, Postcured; ASTM D395B
 33 %
@Temperature 200 °C,
Time 252000 sec
33 %
@Temperature 392 °F,
Time 70.0 hour
Plied, Postcured; ASTM D395B
 34 %
@Temperature 70.0 °C,
Time 252000 sec
34 %
@Temperature 158 °F,
Time 70.0 hour
Plied, no postcure; ASTM D395B
 80 %
@Temperature 150 °C,
Time 252000 sec
80 %
@Temperature 302 °F,
Time 70.0 hour
Plied, no postcure; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature  162 °C
@Time 1800 sec
324 °F
@Time 0.500 hour
Cure
 232 °C
@Time 57600 sec
450 °F
@Time 16.0 hour
Postcure
 
Descriptive Properties
ColorOff whiteUncompounded Viton
FormSheetUncompounded Viton
Formulation as Tested100B303-C
 3MgO
 30MT Black
 6Ca(OH)2
OdorNoneUncompounded Viton
Storage StabilityExcellentUncompounded Viton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® A-201C Fluoroelastomer (FKM)
Chemours Viton® B-435C Fluoroelastomer (FKM)
Chemours Viton® A-HV Fluoroelastomer (FKM)
Chemours Viton® B-601C Fluoroelastomer (FKM)
Chemours Viton® A-361C Fluoroelastomer Compound

PDVC9943 / 170584

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.