MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® A-361C Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Intermediate viscosity level (when compared with Viton® A-201C/Viton® A-401C)
  • Fully precompounded with reduced curative level and Incorporated metal adhesion promoter
  • Improved processing with increased mold flow, easier mold release with less mold fouling, and improved demolding “hot tear”
  • Good metal bonding with standard industrial primers

Applications

  • Compression, transfer, and injection molding of: O-rings and gaskets, Valve stem and crankshaft seals (and other bonded parts requiring fluid and heat resistance of the A-family of Viton®)

    Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/ccUncompounded Viton
Mooney Viscosity 63
@Temperature 121 °C
63
@Temperature 250 °F
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 777724 hours Postcure; ASTM D2240
 7878No Postcure; ASTM D2240
Tensile Strength at Break 9.50 MPa1380 psiNo Postcure; ASTM D412
 14.3 MPa2070 psi24 hours Postcure; ASTM D412
Elongation at Break 213 %213 %24 hours Postcure; ASTM D412
 297 %297 %No Postcure; ASTM D412
100% Modulus  3.80 MPa
@Strain 100 %
551 psi
@Strain 100 %
No Postcure; ASTM D412
 5.50 MPa
@Strain 100 %
798 psi
@Strain 100 %
24 hours Postcure; ASTM D412
Compression Set  7.0 %
@Temperature 23.0 °C,
Time 252000 sec
7.0 %
@Temperature 73.4 °F,
Time 70.0 hour
O-Rings; ASTM D395B
 17 %
@Temperature 200 °C,
Time 252000 sec
17 %
@Temperature 392 °F,
Time 70.0 hour
O-Rings; ASTM D395B
 37 %
@Temperature 232 °C,
Time 252000 sec
37 %
@Temperature 450 °F,
Time 70.0 hour
O-Rings; ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FContinuous use
 >= 260 °C>= 500 °FIntermittent use
Minimum Service Temperature, Air -23.0 - -18.0 °C-9.40 - -0.400 °FViton is generally useful down to -18 to -23°C.
 
Processing PropertiesMetricEnglishComments
Processing Temperature  177 °C
@Time 601 sec
351 °F
@Time 0.167 hour
Slab Cure
 232 °C
@Time 86400 sec
450 °F
@Time 24.0 hour
Postcure
 
Descriptive Properties
ColorOff-whiteUncompounded Viton
FormSlabUncompounded Viton
Formulation as Tested100A361C
 3MgO
 30MT Black
 6Ca(OH)2
OdorNoneUncompounded Viton
Storage StabilityExcellentUncompounded Viton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® A-201C Fluoroelastomer (FKM)
Chemours Viton® A-HV Fluoroelastomer (FKM)
Chemours Viton® B-303C Fluoroelastomer Compound
Chemours Viton® A-401C Fluoroelastomer Compound
Chemours Viton® B-435C Fluoroelastomer (FKM)

PDVC9900 / 170541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.