MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® FDM Nylon 12™ 3D Printing Polymer; Dry
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: FDM® Nylon 12 filament is the 3D printing equivalent of standard industrial PA12 (polyamide 12) material. A strong engineering thermoplastic, it exhibits toughness and high impact strength, without being brittle. Its excellent fatigue properties make it a good option for repetitive-flex applications such as snap-fit clips and closures and press-fit inserts. Other applications include jigs, fixtures and low-volume production parts, as well as accurate prototyping of nylon 12 high-volume injection molded parts. FDM Nylon 12 is available in black.

Mechanical property data from dry samples.

Information provided by Stratasys

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D257
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPaXZ Orientation; ASTM D638
 41.0 MPaZX Orientation; ASTM D638
Tensile Strength, Yield 45.0 MPaZX Orientation; ASTM D638
 50.0 MPaXZ Orientation; ASTM D638
Elongation at Break 6.5 %ZX Orientation; ASTM D638
 30 %XZ Orientation; ASTM D638
Elongation at Yield 5.8 %ZX Orientation; ASTM D638
 6.12 %XZ Orientation; ASTM D638
Modulus of Elasticity 1.20 GPaZX Orientation; ASTM D638
 1.50 GPaXZ Orientation; ASTM D638
Flexural Strength 55.0 MPa
@Strain 5.0 %
XZ Orientation; ASTM D790, Procedure A
 55.0 MPa
@Strain 5.0 %
ZX Orientation; ASTM D790, Procedure A
Compressive Modulus 1.48 GPaXZ Orientation; ASTM D695
 1.65 GPaZX Orientation; ASTM D695
Izod Impact, Notched 70.0 J/mZX Orientation; ASTM D256, ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.5
@Frequency 2.00e+6 Hz
XY, XZ/ZX Orientations; ASTM D150
 2.87
@Frequency 1000 Hz
XZ/ZX Orientation; ASTM D150
 3.11
@Frequency 1000 Hz
XY Orientation; ASTM D150
Dissipation Factor 0.0080
@Frequency 2.00e+6 Hz
XZ/ZX Orientation; ASTM D150
 0.0090
@Frequency 1000 Hz
XZ/ZX Orientation; ASTM D150
 0.014
@Frequency 2.00e+6 Hz
XY Orientation; ASTM D150
 0.066
@Frequency 1000 Hz
XY Orientation; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 70.0 - 95.0 °C
XZ/ZX Orientation; ASTM E831
 85.0 µm/m-°C
@Temperature -50.0 - 10.0 °C
XY, XZ/ZX Orientations; ASTM E831
 95.0 µm/m-°C
@Temperature 10.0 - 50.0 °C
XY, XZ/ZX Orientations; ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CXZ/ZX Orientation; ASTM D648 Method B
 95.0 °CXY Orientation; ASTM D648 Method B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CXZ/ZX Orientation; ASTM D648 Method B
 85.0 °CXY Orientation; ASTM D648 Method B
Glass Transition Temp, Tg 35.0 °CInflection Point, XY, XZ/ZX; ASTM D7426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® FDM Nylon 12™ 3D Printing Polymer; Conditioned
Stratasys® ABS-M30
Stratasys® PC-ABS
Celanese Celstran® PA66-GF50-02-US Nylon 66, 50% Glass Reinforced
Overview of materials for Nylon 12

PSTRAT105 / 206202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.