MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Materion AMC4632 Aluminum Silicon Alloy, T6  (discontinued **)
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: AMC4632 is a high quality hyper-eutectic aluminum-silicon alloy. It is manufactured by a powder metallurgy route to refine the microstructure and provide enhanced mechanical properties. This alloy offers a high tensile modulus (approximately 15% higher than AA4032), good strength and excellent fatigue resistance at ambient and elevated temperatures. It can be used as a replacement for conventional aluminum alloys such as AA4032 and AA2618 in a range of applications. AMC4632 may be machined to fine surface finish and tolerances using high speed techniques.

Typical mechanical property data for cold water quenched T6 samples.

Information supplied by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.70 g/cc0.0975 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 440 MPa63800 psiBillet or Forging
 460 MPa66700 psiExtrusion, Longitudinal Value
Tensile Strength, Yield  375 MPa
@Strain 0.2 %
54400 psi
@Strain 0.2 %
Forging
 390 MPa
@Strain 0.2 %
56600 psi
@Strain 0.2 %
Billet
 395 MPa
@Strain 0.2 %
57300 psi
@Strain 0.2 %
Extrusion, Longitudinal Value
Elongation at Break 1.1 %1.1 %Billet
 1.5 %1.5 %Forging
 2.5 %2.5 %Extrusion, Longitudinal Value
Modulus of Elasticity 94.0 GPa13600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000690 ohm-cm0.00000690 ohm-cmT1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.1 µm/m-°C8.94 µin/in-°F
Thermal Conductivity 129 W/m-K895 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alcoa Deltalloy® 4032-T651 Aluminum
Aluminum 4032-O
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Forged Plate
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Forged Plate
Materion SupremEX® 225XE Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Forged Plate

NBB975 / 192256

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.