MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber, 5% Filler by Weight/Unspecified Filler\Reinfor

Features: Conductive

TPCI# 9117116

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 3.17 mm
0.0080 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
4.0 g/10 min
@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.4 MPa3100 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Flexural Strength 29.0 MPa4200 psiASTM D790
Flexural Modulus 1.65 GPa240 ksiASTM D790
Izod Impact, Notched 2.14 J/cm
@Thickness 3.17 mm
4.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D257
Surface Resistance <= 1.00e+6 ohm<= 1.00e+6 ohmASTM D257
Static Decay <= 2.0 sec<= 2.0 secMIL B-81705C
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C200 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene, Carbon Fiber Filled
Buckeye Polymers BP RPP 1009 GK Polypropylene, 10% Glass Filled
Multibase Multi-Pro® 2012 RC 20% Glass Filled Polypropylene
EPICHEM Epilen PP 20GF NAT Polypropylene, 20% Glass Fiber

PTPC0917 / 136855

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.