MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.872 - 1.68 g/cc0.0315 - 0.0607 lb/in³Average value: 1.06 g/cc Grade Count:43
Filler Content 1.00 - 50.0 %1.00 - 50.0 %Average value: 21.5 % Grade Count:18
Water Absorption 0.0100 - 0.0500 %0.0100 - 0.0500 %Average value: 0.0200 % Grade Count:8
Additive Loading 10.0 - 50.0 %10.0 - 50.0 %Average value: 30.0 % Grade Count:5
Maximum Moisture Content  0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000500 - 0.0150 cm/cm0.000500 - 0.0150 in/inAverage value: 0.00374 cm/cm Grade Count:25
Linear Mold Shrinkage, Transverse 0.00200 - 0.0105 cm/cm0.00200 - 0.0105 in/inAverage value: 0.00517 cm/cm Grade Count:3
Melt Flow 1.10 - 25.0 g/10 min1.10 - 25.0 g/10 minAverage value: 10.2 g/10 min Grade Count:11
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 19.3 - 165 MPa2800 - 23900 psiAverage value: 63.6 MPa Grade Count:44
Tensile Strength, Yield 22.0 - 43.4 MPa3190 - 6290 psiAverage value: 31.8 MPa Grade Count:3
Elongation at Break 0.400 - 436 %0.400 - 436 %Average value: 22.0 % Grade Count:41
Modulus of Elasticity 1.03 - 27.6 GPa150 - 4000 ksiAverage value: 11.7 GPa Grade Count:34
Flexural Yield Strength 27.6 - 260 MPa4000 - 37700 psiAverage value: 103 MPa Grade Count:37
Flexural Modulus 1.48 - 20.0 GPa215 - 2900 ksiAverage value: 9.29 GPa Grade Count:40
Izod Impact, Notched 0.280 - 3.20 J/cm0.525 - 6.00 ft-lb/inAverage value: 1.20 J/cm Grade Count:27
Izod Impact, Unnotched 1.07 - 11.2 J/cm2.00 - 21.0 ft-lb/inAverage value: 3.89 J/cm Grade Count:23
Izod Impact, Notched (ISO) 1.00 - 9.00 kJ/m²0.476 - 4.28 ft-lb/in²Average value: 5.75 kJ/m² Grade Count:4
 4.00 - 6.00 kJ/m²
@Temperature -30.0 - -30.0 °C
1.90 - 2.86 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 5.33 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 35.0 - 44.0 kJ/m²
@Temperature -30.0 - -30.0 °C
16.7 - 20.9 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 39.5 kJ/m² Grade Count:2
Charpy Impact Unnotched 2.00 - 3.50 J/cm²9.52 - 16.7 ft-lb/in²Average value: 3.00 J/cm² Grade Count:3
 1.50 - 1.50 J/cm²
@Temperature -30.0 - -30.0 °C
7.14 - 7.14 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.240 - 2.00 J/cm²1.14 - 9.52 ft-lb/in²Average value: 0.914 J/cm² Grade Count:13
 0.400 - 2.00 J/cm²
@Temperature -40.0 - -30.0 °C
1.90 - 9.52 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 0.967 J/cm² Grade Count:3
Puncture Energy  5.40 - 6.20 J
@Temperature -20.0 - 0.000 °C
3.98 - 4.57 ft-lb
@Temperature -4.00 - 32.0 °F
Average value: 5.80 J Grade Count:1
 5.40 - 6.20 J
@Thickness 3.00 - 3.00 mm
3.98 - 4.57 ft-lb
@Thickness 0.118 - 0.118 in
Average value: 5.80 J Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.100 - 3.10e+9 ohm-cm0.100 - 3.10e+9 ohm-cmAverage value: 1.57e+8 ohm-cm Grade Count:24
Surface Resistance 100 - 1.00e+13 ohm100 - 1.00e+13 ohmAverage value: 8.07e+11 ohm Grade Count:25
Static Decay 0.500 - 2.00 sec0.500 - 2.00 secAverage value: 1.50 sec Grade Count:9
 
Thermal PropertiesMetricEnglishComments
CTE, linear 36.0 - 100 µm/m-°C20.0 - 55.6 µin/in-°FAverage value: 56.4 µm/m-°C Grade Count:3
Melting Point 163 - 165 °C325 - 329 °FAverage value: 164 °C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 132 - 292 °C270 - 558 °FAverage value: 162 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 162 °C140 - 324 °FAverage value: 127 °C Grade Count:22
Vicat Softening Point 80.0 - 155 °C176 - 311 °FAverage value: 121 °C Grade Count:8
Flammability, UL94 HBHBGrade Count:15
 
Processing PropertiesMetricEnglishComments
Processing Temperature 188 - 227 °C370 - 440 °FAverage value: 209 °C Grade Count:8
Nozzle Temperature 200 - 270 °C392 - 518 °FAverage value: 225 °C Grade Count:12
Melt Temperature 160 - 270 °C320 - 518 °FAverage value: 217 °C Grade Count:25
Mold Temperature 30.0 - 90.0 °C86.0 - 194 °FAverage value: 56.7 °C Grade Count:33
Injection Velocity 20.0 - 76.2 mm/sec0.787 - 3.00 in/secAverage value: 56.4 mm/sec Grade Count:4
Drying Temperature 70.0 - 120 °C158 - 248 °FAverage value: 83.6 °C Grade Count:19
Injection Pressure 30.0 - 103 MPa4350 - 15000 psiAverage value: 83.8 MPa Grade Count:17
Cushion 0.635 cm0.250 inAverage value: 0.635 cm Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Overview of materials for Polypropylene with Carbon Black Filler
Overview of materials for Polypropylene with 40% Glass Fiber Filler

O4721 / 78385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.