MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Luran® S 776SE ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Luran® S 776SE is suitable extrusion applications. It provides good impact toughness and enables matte surface appearance for extruded sheets. Good impact strength, Suitable for extrusion, Enables matte surface finish in extrusion. Applications: sheets, gardening equipment.

Key Words: S 776 SE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.590 g/ccwith external lubricant
Density 1.07 g/ccISO 1183
Moisture Absorption at Equilibrium 0.35 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 1.65 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cmISO 294-4
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 89ASTM Test
Hardness, Shore D 67ISO 868
Ball Indentation Hardness 70.0 MPaISO 2039-1
Tensile Strength, Yield 47.0 MPaISO 527
Elongation at Break 12 %ISO 527
Elongation at Yield 3.3 %ISO 527
Tensile Modulus 2200 MPaISO 527
Flexural Strength 65.0 MPaISO 178
Izod Impact, Notched 0.510 J/cm
@Temperature -40.0 °C
ASTM Test
 2.60 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 30.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2000 MPaISO 899
Tensile Creep Modulus, 1000 hours 1200 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0090
@Frequency 100 Hz
IEC 60250
 0.034
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 - 110 µm/m-°CISO 11359
Thermal Conductivity 0.170 W/m-KDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 101 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 92.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 104 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze <= 2.0 %ASTM D1003
Transmission, Visible 89 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
 
Compliance PropertiesOriginal ValueComments
NSF NoNSF Std. 51
 NoNSF Std. 61
USP Class VI No
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedYes
Injection Molding Regrind<30%
Primary Processing TechniqueExtrusion
ProcessingBlow Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
Special characteristicHeat stabilized or stable to heat
 Light stabilized or stable to light
 U.V. stabilized or stable to weather
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 776 S UV ASA
INEOS Styrolution Luran® S 777K ASA
INEOS Styrolution Luran® S 757G ASA
INEOS Styrolution Luran® S 797SE ASA
INEOS Styrolution Luran® S 778T ASA

PBASF9004 / 84768

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.