MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Luran® S 776SE ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Luran® S 776SE is suitable extrusion applications. It provides good impact toughness and enables matte surface appearance for extruded sheets. Good impact strength, Suitable for extrusion, Enables matte surface finish in extrusion. Applications: sheets, gardening equipment.

Key Words: S 776 SE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.590 g/cc0.0213 lb/in³with external lubricant
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.35 %
@Temperature 23.0 °C
0.35 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation 1.65 %
@Temperature 23.0 °C
1.65 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm0.0050 - 0.0090 in/inISO 294-4
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8989ASTM Test
Hardness, Shore D 6767ISO 868
Ball Indentation Hardness 70.0 MPa10200 psiISO 2039-1
Tensile Strength, Yield 47.0 MPa6820 psiISO 527
Elongation at Break 12 %12 %ISO 527
Elongation at Yield 3.3 %3.3 %ISO 527
Tensile Modulus 2.20 GPa319 ksiISO 527
Flexural Strength 65.0 MPa9430 psiISO 178
Izod Impact, Notched 0.510 J/cm
@Temperature -40.0 °C
0.955 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 2.60 J/cm
@Thickness 3.17 mm
4.87 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2000 MPa290000 psiISO 899
Tensile Creep Modulus, 1000 hours 1200 MPa174000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0090
@Frequency 100 Hz
0.0090
@Frequency 100 Hz
IEC 60250
 0.034
@Frequency 1e+6 Hz
0.034
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C205 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  92.0 °C
@Load 5.10 kg
198 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 104 °C
@Load 1.02 kg
219 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 2.0 %<= 2.0 %ASTM D1003
Transmission, Visible 89 %
@Wavelength 550 nm
89 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
 
Compliance PropertiesMetricEnglishComments
NSF NoNoNSF Std. 51
 NoNoNSF Std. 61
USP Class VI NoNo
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedYes
Injection Molding Regrind<30%
Primary Processing TechniqueExtrusion
ProcessingBlow Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
Special characteristicHeat stabilized or stable to heat
 Light stabilized or stable to light
 U.V. stabilized or stable to weather
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 776 S UV ASA
INEOS Styrolution Luran® S 777K ASA
INEOS Styrolution Luran® S 757G ASA
INEOS Styrolution Luran® S 797SE ASA
INEOS Styrolution Luran® S 778T ASA

PBASF9004 / 84768

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.