MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 3092/65 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid silicone rubber ELASTOSIL® LR 3092/65 A/B is a paste-like two-component compound with short curing times. The vulcanizates are noted for good mechanical properties and for excellent heat resistance within a temperature range of -55 °C to +230 °C, and for a short time up to +300 °C. Outstanding low compression sets can be achieved after post curing.

Application: ELASTOSIL® LR 3092/65 A/B is particularly suitable for the economical production of large series of articles for the automotive industry, e. g. inter cooler gaskets.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183-1 A
Viscosity 1.70e+6 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 66DIN 53505
Tensile Strength at Break 9.90 MPaDIN 53504 S 1
Elongation at Break 320 %DIN 53504 S 1
Tear Strength 25.0 kN/mASTM 624 B
Compression Set 8.0 %
@Temperature 175 °C,
Time 79200 sec
post cure 6h/200°C; DIN ISO 815-B
 10 %
@Temperature 175 °C,
Time 79200 sec
post cure 4h/210°C; DIN ISO 815-B
 16 %
@Temperature 200 °C,
Time 79200 sec
post cure 4h/210°C; DIN ISO 815-B
 24 %
@Temperature 200 °C,
Time 79200 sec
post cure 6h/200°C; DIN ISO 815-B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 230 °C
 300 °Cshort term
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
postcuring for 4h/200°C (in ventilated air)
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9146 / 204675

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.