MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wacker Elastosil® LR 3092/65 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid silicone rubber ELASTOSIL® LR 3092/65 A/B is a paste-like two-component compound with short curing times. The vulcanizates are noted for good mechanical properties and for excellent heat resistance within a temperature range of -55 °C to +230 °C, and for a short time up to +300 °C. Outstanding low compression sets can be achieved after post curing.

Application: ELASTOSIL® LR 3092/65 A/B is particularly suitable for the economical production of large series of articles for the automotive industry, e. g. inter cooler gaskets.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183-1 A
Viscosity 1.70e+6 cP
@Shear Rate 0.900 1/s
1.70e+6 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6666DIN 53505
Tensile Strength at Break 9.90 MPa1440 psiDIN 53504 S 1
Elongation at Break 320 %320 %DIN 53504 S 1
Tear Strength 25.0 kN/m143 pliASTM 624 B
Compression Set  8.0 %
@Temperature 175 °C,
Time 79200 sec
8.0 %
@Temperature 347 °F,
Time 22.0 hour
post cure 6h/200°C; DIN ISO 815-B
 10 %
@Temperature 175 °C,
Time 79200 sec
10 %
@Temperature 347 °F,
Time 22.0 hour
post cure 4h/210°C; DIN ISO 815-B
 16 %
@Temperature 200 °C,
Time 79200 sec
16 %
@Temperature 392 °F,
Time 22.0 hour
post cure 4h/210°C; DIN ISO 815-B
 24 %
@Temperature 200 °C,
Time 79200 sec
24 %
@Temperature 392 °F,
Time 22.0 hour
post cure 6h/200°C; DIN ISO 815-B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 230 °C446 °F
 300 °C572 °Fshort term
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
postcuring for 4h/200°C (in ventilated air)
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9146 / 204675

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.