MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company ESD C 1200 T-70D Ether-based Thermoplastic Polyurethane Elastomer; Electrically Conductive - ESD Protection
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D 792
Linear Mold Shrinkage 0.0070 - 0.015 cm/cm
@Thickness 3.20 mm
0.0070 - 0.015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575instantaneous; ASTM D 2240
Tensile Strength at Break 27.6 MPa
@Thickness 3.20 mm
4000 psi
@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Elongation at Break 100 %
@Thickness 3.20 mm
100 %
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 140 kN/m800 pliDie C; ASTM D 624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D 257
Surface Resistance <= 1e+05<= 1e+05ESD STM11.11
Surface Resistivity per Square <= 1.00e+6 ohm<= 1.00e+6 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 218 °C365 - 425 °F
Mold Temperature 37.8 - 60.0 °C100 - 140 °F
Drying Temperature 107 °C
@Time 21600 sec
225 °F
@Time 6.00 hour
Moisture Content 0.010 %0.010 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer
Taiwan Sheen Soon Sheenthane® D6610 Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer
RTP Company RTP 1200 T-80A Ether-based Thermoplastic Polyurethane Elastomer
RTP Company RTP 1200 S-60D Ester-based Thermoplastic Polyurethane Elastomer

PQZUA7272 / 134907

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.