MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1200 T-80A Ether-based Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D 792
Linear Mold Shrinkage 0.010 cm/cm
@Thickness 3.17 mm
0.010 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 828210 s delay; ASTM D 2240
Tensile Strength at Break 31.0 MPa4500 psiASTM D 412
Tensile Stress at Strain  4.14 MPa
@Strain 50 %
600 psi
@Strain 50 %
ASTM D 412
 5.52 MPa
@Strain 100 %
800 psi
@Strain 100 %
ASTM D 412
 11.7 MPa
@Strain 300 %
1700 psi
@Strain 300 %
ASTM D 412
Elongation at Break 600 %600 %ASTM D 412
Tear Strength 96.4 kN/m550 pliDie C; ASTM D 624
Compression Set 30 %
@Temperature 23.0 °C,
Time 79200 sec
30 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 216 °C360 - 420 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Drying Temperature 82.2 °C180 °F
Dry Time 6 hour6 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 27.6 - 55.2 MPa4000 - 8000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1200 S-60D Ester-based Thermoplastic Polyurethane Elastomer
RTP Company RTP 1200 S-80A Ester-based Thermoplastic Polyurethane Elastomer
RTP Company RTP 1200 S-75A Ester-based Thermoplastic Polyurethane Elastomer
RTP Company RTP 1200 S-65D Ester-based Thermoplastic Polyurethane Elastomer
RTP Company RTP 1200 S-85A Precolor Ester-based Thermoplastic Polyurethane Elastomer

PQZWA4196 / 91860

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.