Characteristics: - Good dielectric properties
- High mechanical strength
- Good dimensional stability
- Good oxidative stability
- Inherent flame retardance
- Good hydrolytic stability
Applications: - Printer cartridges
- Mobile phone parts
- Surgical tool trays
- Dental cases
- Business machine parts
- Alkaline battery cell cases
- Household appliances
Information provided by Gharda. Solvay Advanced Polymers completed its acquisition of this product line in May 2006. |