MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast/AboCure 8109-13
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Liquid hardener version of AboCast/AboCure 8109-11.

Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45 min/100°C (212°F), 30 mins/140°C (285°F), 15 min+1-3h/180°C (355°F).

Applications: Potting and laminating.

Key Words: potting, laminating, laminates
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Water Absorption 0.30 - 0.40 %0.30 - 0.40 %(60x10X4 mm bar) after 1 hour at 100°C (212°F)
 0.40 - 0.50 %0.40 - 0.50 %(60x10X4 mm bar) after 10 days at 20°C (77°F)
Viscosity  1000 - 2000 cP
@Temperature 40.0 °C
1000 - 2000 cP
@Temperature 104 °F
 10000 - 15000 cP
@Temperature 21.0 °C
10000 - 15000 cP
@Temperature 69.8 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 68.95 MPa10000 psi
Modulus of Elasticity 3.447 GPa500.0 ksi
Flexural Yield Strength 137.9 MPa20000 psi
Compressive Yield Strength 151.7 MPa22000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.50e+16 ohm-cm>= 1.50e+16 ohm-cm
Dielectric Constant  3.9 - 4.4
@Frequency 1e+6 Hz
3.9 - 4.4
@Frequency 1e+6 Hz
 4.2 - 4.5
@Frequency 50 Hz
4.2 - 4.5
@Frequency 50 Hz
Dielectric Strength 15.7 - 17.7 kV/mm
@Thickness 3.17 mm
400 - 450 kV/in
@Thickness 0.125 in
Short time value
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 - 55.0 µm/m-°C
@Temperature 20.0 °C
27.8 - 30.6 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 150 °C302 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °F
Pot Life  30.0 - 60.0 min
@Temperature 60.0 °C
30.0 - 60.0 min
@Temperature 140 °F
 60.0 - 180 min
@Temperature 40.0 °C
60.0 - 180 min
@Temperature 104 °F
 180 - 300 min
@Temperature 20.0 °C
180 - 300 min
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay BR® 4535A Paste Adhesive
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications
Hybrid Plastics POSS® EP 1000 Epoxy Adhesive
Henkel Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill

PABFB1 / 22027

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.