MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hybrid Plastics POSS® EP 1000 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: EP1000 is a POSS® based epoxy adhesive with outstanding oxidative resistance to ozone, plasma, or atomic oxygen environments. The EP1000 POSS® Epoxy is also well-suited for peroxide and steam. It provides an exceptional transparent adhesive in these conditions for metallic, molded plastic and composite materials.

Information provided by Hybrid Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³after cure
Viscosity <= 5000 cP<= 5000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8580 - 85
Modulus of Elasticity 3.00 - 3.50 GPa435 - 508 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
27.8 µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg 100 - 110 °C212 - 230 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 6.00 min
@Temperature 80.0 °C
0.100 hour
@Temperature 176 °F
Pot Life 180 min180 min
Shelf Life 6.00 - 12.0 Month6.00 - 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay BR® 4535A Paste Adhesive
Master Bond Supreme 10HTS Silver Filled Electrically Conductive One Part Epoxy
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications
Henkel Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill

PHYBR029 / 78839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.