(Viewing data as-entered.
Click here
to return)
Sumitomo Bakelite Durez® 14798 Phenolic Resin
Categories:
Polymer
;
Thermoset
;
Phenolic
Material Notes:
Durez 14798 is a liquid one-step phenolic resin. Durez 14798 has a medium viscosity, a medium cure, and a rigid set.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Volatiles
30 %
DCT 4005A-1
pH
7.0
DCT 4064A
Viscosity Measurement
5500
DCT 4003H
Descriptive Properties
Appearance
Reddish Liquid
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Sumitomo Bakelite SUMILITERESIN® PR-55170 Powder phenolic resin
Sumitomo Bakelite SUMILITERESIN® PR-51992 Solid phenolic resin
Sumitomo Bakelite SUMILITERESIN® PR-310 Powder phenolic resin
Sumitomo Bakelite SUMILITERESIN® PR-13349 Phenolic resin
PSUMIT227 / 194032
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.