MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sumitomo Bakelite SUMILITERESIN® PR-51992 Solid phenolic resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: SUMILITERESIN ®PR-51992 is a solid novolac resin based on a modified novolac polymer. It is supplied in the form of flakes for compounds.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 8585[mm²/s/50%EtOH, 25°C]
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.0 °C185 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 1.42 min
@Temperature 165 °C
1.42 min
@Temperature 329 °F
 
Descriptive Properties
AppearanceSlightly Brown Flakes
Flow Distance75mm, 125°C
Free Phenol, GC, %3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite SUMILITE® PLC-2147 AQ Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 RF Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 GSSM Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 GF Paper Phenolic
Sumitomo Bakelite Plyophen 43575 Phenolic Resin

PSUMIT616 / 194421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.