Product Description: Celanex 2002SW1 Natural is an unreinforced PTFE-modified PBT with improved friction, sliding, and wear properties. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Processing Method: Injection Molding Information provided by Celanese |