MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Toyobo Celanex® 2002SW1 PBT, PTFE modified
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Product Description: Celanex 2002SW1 Natural is an unreinforced PTFE-modified PBT with improved friction, sliding, and wear properties.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.20 %0.20 %Equilibrium, 50% RH; ISO 62
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.017 - 0.021 cm/cm0.017 - 0.021 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.016 - 0.019 cm/cm0.016 - 0.019 in/inISO 294-4
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 250 °C
21 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 56.0 MPa8120 psiISO 527-2/50
Elongation at Break 19 %19 %Nominal; ISO 527-2/50
Elongation at Yield 7.0 %7.0 %ISO 527-2/50
Tensile Modulus 2.60 GPa377 ksiISO 527-1
Charpy Impact, Notched 0.336 J/cm²1.60 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FISO 11357-3
Glass Transition Temp, Tg 60.0 °C140 °FISO 11357-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °FHopper
 250 - 260 °C482 - 500 °FHot Runner
Feed Temperature 230 - 240 °C446 - 464 °FInjection
Rear Barrel Temperature 230 - 240 °C446 - 464 °F
Middle Barrel Temperature 235 - 250 °C455 - 482 °F
Front Barrel Temperature 235 - 250 °C455 - 482 °F
Nozzle Temperature 250 - 260 °C482 - 500 °F
Zone 4 240 - 260 °C464 - 500 °FInjection
Melt Temperature 235 - 260 °C455 - 500 °F
Mold Temperature 65.0 - 92.8 °C149 - 199 °F
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6167 / 310860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.