MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, and Sand.

Applications: General-utility bearings and bushings, automobile fittings.

Classified under: High-leaded tin bronzes. ASTM B584; formerly ASTM B144-3B

Typical data for sand-cast test bars. Alloy does not respond to heat treating

Key Words: High lead tin bronze, ASTM B584, ASTM B144-3B, SAE 660
Vendors: Dura-Bar Metal Services is a major distributor of bronze alloys. We stock a large inventory of C93200 in tubes and rounds. Our customers rely on us for high quality materials that help increase their profitability. Call us at 1-800-526-0548 or visit dura-barms.com for more information.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.93 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 65
Tensile Strength, Ultimate 240 MPa
Tensile Strength, Yield 125 MPa
@Strain 0.5 %
Elongation at Break 20 %in 50 mm
Modulus of Elasticity 100 GPa
Compressive Strength 315 MPaat permanent set of 10%
Fatigue Strength 110 MPa
@# of Cycles 1.00e+8
rotating beam
Machinability 70 %UNS C36000 (free-cutting brass) = 100%
Izod Impact 8.00 J
Coefficient of Friction 0.10
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 0.000 - 100 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 59.0 W/m-K
@Temperature 20.0 °C
Melting Point 315 °CIncipient
 855 - 975 °C
Solidus 855 °C
Liquidus 975 °C
Shrinkage 1.8 %Patternmaker's Shrinkage (7/32 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 260 °CStress-Relieving Temperature
 
Component Elements PropertiesOriginal ValueComments
Antimony, Sb <= 0.35 %
Copper, Cu 81 - 85 %
Iron, Fe <= 0.20 %
Lead, Pb 6.0 - 8.0 %
Nickel, Ni <= 0.50 %
Phosphorus, P <= 0.15 %
Silicon, Si <= 0.0030 %
Sulfur, S <= 0.080 %
Tin, Sn 6.3 - 7.5 %
Zinc, Zn 2.0 - 4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Oilite® Bronze Bearing Alloy - SAE 841
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper
MetalTek MTEK 83-7-7-3 Cast UNS C93200 Bearing Bronze
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Sand Cast

MC93200b1 / 11945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.