BMC LPA 240/20 NEUTRO is a bulk molding compound based on an unsaturated polyester resin class “A” grade reinforced with glass fibers. This BMC has been developed for body panel application, with excellent varnish adhesion and excellent surface. BMC LPA 240/20 NEUTRO is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.Information provided by Polynt Composites. |