MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott MAZ 8 UV Bandpass Filter (Spectral range 200 – 333 nm)
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Spectral range 220 – 333 nm, +/- 0.5%

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 465 - 485 microns18.3 - 19.1 mil
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °Fcontinuous
 100 °C212 °Fintermittent
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 0.0010 %
@Wavelength 380 - 600 nm
>= 0.0010 %
@Wavelength 380 - 600 nm
UV Transmittance  >= 0.0010 %
@Wavelength 333 - 380 nm
>= 0.0010 %
@Wavelength 333 - 380 nm
 <= 15 %
@Wavelength 220 - 333 nm
<= 15 %
@Wavelength 220 - 333 nm
 
Descriptive Properties
Blocking rangeUnlimited
Half width (FWHM)6-10 nm
Q=(tenth width/half width)1.75
q=(thousandth width/half width)4.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning Vycor® 7913 UV-Transmitting Glass
Corning Vycor® 7907 UV-Blocking Glass
Schott KMD 12 UV Bandpass Filter (Spectral range 200 – 333 nm)
Schott DAD 8-70 UV, VIS, and Near IR Bandpass Filter
Overview of materials for Polycarbonate, UV Stabilized

CSGT9803 / 183056

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.