MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Specialty Materials Boron Monofilament, 5.6 mil (142 µm) diameter
Categories: Metal; Other Engineering Material; Composite Fibers; Pure Element

Material Notes: Exceptional modulus and compressive strength. The Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source. Elemental boron is deposited on a fine tungsten wire substrate and produced in diameters of 4.0-mil (102-micron) and 5.6-mil (142-micron). The resulting fiber is essentially amorphous boron with a fully borided-tungsten core. The textured surface provides an excellent interface in resin matrix composites, eliminating any need for sizing treatments. Primarily used in resin-matrix composites

Information provided by Specialty Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.38 g/cc0.0860 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 32003200
Tensile Strength, Ultimate 4000 MPa580000 psi
Modulus of Elasticity 400 GPa58000 ksitension
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 250 ohm-cm250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.50 µm/m-°C
@Temperature 20.0 °C
2.50 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°F
Thermal Conductivity 25.0 W/m-K174 BTU-in/hr-ft²-°Fbulk boron
Melting Point 2300 °C4170 °F
Maximum Service Temperature, Air 500 °C932 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 100 %100 %
 
Descriptive Properties
Cross-SectionRound
Length> 2400 m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBORON00a / 287749

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.