MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik REWOPHAT® EAK 8190 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: REWOPHAT® EAK 8190 is a lauryl polyglycol ether phosphoric acid ester.

Application: REWOPHAT® EAK 8190 is used as an extreme pressure (EP) and antiwear additive (AW) in aqueous based metal working fluids (MWF). It improves lubricity in neat rolling and drawing oils. Furthermore, REWOPHAT® EAK 8190 is used in the plastic and textile industry as an emulsifier and antistatic agent.

Properties / Benefits:

  • REWOPHAT® EAK 8190 provides good EP/AW properties in aqueous based MWF.
  • REWOPHAT® EAK 8190 enhances lubricity in neat rolling and drawing oils.
  • REWOPHAT® EAK 8190 has good hydrolytic stability in slightly acidic to alkaline solutions.
  • REWOPHAT® EAK 8190 is 73 % readily biodegradable (OECD 301 E).

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 1.0 - 3.01.0 - 3.0
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 140 - 160140 - 160[mg KOH/g]
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.5 %<= 1.5 %
 
Descriptive Properties
Appearanceyellow, clear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Laurel BioComposite Bio-Res™ 20% Composite in HDPE
Eastman Optifilm™ 300 Enhancer
BYK Necowel FLE 55N Clay Additive

PEVONIL511 / 196715

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.