MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Krytox® FG 35 Anticorrosion Food Grade Grease  (discontinued **)
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE); PTFE Gellant

Material Notes: Krytox® anticorrosion greases are high temperature, extreme pressure, water-resistant greases for your most demanding needs. They provide stable performance in temperature extremes and are designed to reduce friction and wear while extending equipment life in severe duty applications. They are extremely resistant to water washout and give long-term rust and corrosion protection for bearings and other equipment. Their wide temperature range allows them to be used in both high and low temperature applications. The superior film-forming capability of Krytox® lubricants provides a thicker oil layer and reduces wear. The nonoxidizing nature of the oils makes the greases last longer. The oils don’t gum up as they age, so they won’t harden the greases and cause catastrophic failure. These greases have superior extreme pressure properties and excellent adhesion, so they stand up to all conditions. Krytox® anticorrosion greases are recommended for use in food and packaging equipment where an H-1 rated lubricant is required. There are several grades available to meet a variety of temperature conditions; all contain antirust additives. Krytox® FG anticorrosion greases are now available for use in food applications where a lubricant with an H-1 rating is required. The product line includes several different types of greases with and without additives and a range of oils for all types of systems. Krytox® lubricants are commonly used in aerospace, automotive, industrial, and semiconductor applications, as well as solving many other routine lubrication problems.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015. This specific product was discontinued prior to the formation of Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 149Viscosity Index
Kinematic Viscosity at 40°C (104°F) 500 cSt
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °C
Minimum Service Temperature, Air -20.0 °C
 
Descriptive Properties
ColorWhite, Creamy Consistency
NLGI Grade2
Rust PreventionPassASTM D-1743

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nye Lubricants UniFlor 8511U (UF) Synthetic Oil
Nye Lubricants FTL-9000 Grease
Nye Lubricants 9704S Grease
Nye Lubricants 876M-MS FG) Grease
Chemours Krytox® XHT-ACX PFPE Grease

WDUPK06 / 75366

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.