MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nye Lubricants FTL-9000 Grease
Categories: Fluid; Lubricant; PTFE Gellant

Material Notes: Information provided by Nye Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity at 40°C (104°F) 700 cSt700 cStBase Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 17 cSt17 cStBase Oil; ASTM D445
Evaporation Loss 1.3 %1.3 %24 hrs, 100C; ASTM D972
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 179179ASTM D217
Oil Separation 0.00 %0.00 %24 hrs, 100C; FTM 719B, 321.2
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °FRecommended
Minimum Service Temperature, Air 10.0 °C50.0 °FRecommended
Pour Point 5.00 °C41.0 °FBase Oil; ASTM D97
 
Descriptive Properties
Base Fluid TypeCTFE
Gellant TypePTFE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nye Lubricants 9704S Grease
Nye Lubricants 876M-MS FG) Grease
Chemours Krytox® XHT-ACX PFPE Grease
Chemours Krytox® XHT-AC PFPE Grease
Chemours Krytox® FG 35 Anticorrosion Food Grade Grease

WNYE555 / 76849

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.