MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChevronTexaco ATF+3® Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: General Description

DaimlerChrysler has had their own ATF specifications for many years, but as of 1997, Chrysler owners manuals no longer list DEXRON as an acceptable replacement. ATF+3 is a readily available mineral oil-based ATF that is suitable in any application calling for ATF PLUS® , ATF+2® , or a Type 7176® fluid. Vehicles manufactured after 1999 require ATF+4® , a synthetic-based ATF only available through DaimlerChrysler.

Chevron ATF+3 is specially formulated to optimize performance of Chrysler transmissions and transaxles.

Applications

Chevron ATF+3 Automatic Transmission Fluid is designed for use in all Chrysler automatic transmissions and automatic transaxles where a Mopar ATF PLUS, ATF+2 or ATF+3 fluid is specified.

It is not recommended for use in transmissions specifying either DEXRON® or MERCON® type fluids

Chevron ATF+3 Automatic Transmission Fluid has been registered with the Chrysler Corporation.

Key Words: CPS Number: 238200; MSDS Number: 6801
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31.2 °
Brookfield Viscosity 18000 cP
@Temperature -40.0 °C
Viscosity Measurement 188Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 35.9 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.6 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °CASTM D97
Flash Point 194 °CASTM D92
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sylvin Technologies 8960-60 Natural PVC Extrusion Compound
Solvay Chemicals NOCOLOK® Thickener (water soluble)
Sandvik DH45 Cemented Carbide for Woodworking
Novatec Novablend® 5021 PVC

WCHEV040 / 74655

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.