MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Radel® RG-5010 Polyphenylsulfone (PPSU)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Radel RG-5010 is a 10% glass-fiber reinforced polyphenylsulfone (PPSU). Compared to unreinforced polyphenylsulfone, this grade has increased strength, stiffness and creep resistance. This resin is particularly well suited for applications where excellent durability after long-term heat, hot water, or steam exposure is required. - Blue: Radel RG-5010 BU 323

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
Filler Content 10 %Glass Fiber Reinforcement
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
Water Absorption at Saturation 0.50 %ASTM D570
Linear Mold Shrinkage, Flow 0.0010 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cmASTM D955
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 365 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 85.0 MPa
@Thickness 3.18 mm
Injection Molded; ASTM D638
Elongation at Break 7.0 %
@Thickness 3.18 mm
Injection Molded; ASTM D638
Tensile Modulus 3700 MPa
@Thickness 3.18 mm
Injection Molded; ASTM D638
Flexural Strength 144 MPa
@Thickness 3.18 mm
Injection Molded; ASTM D790
Flexural Modulus 3380 MPa
@Thickness 3.18 mm
ASTM D790
Izod Impact, Notched 75.0 J/m
@Thickness 3.18 mm
Injection Molded; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 7.00e+15 ohm-cm
@Thickness 3.18 mm
ASTM D257
Dielectric Constant 3.41
@Thickness 3.18 mm,
Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
@Thickness 3.18 mm
ASTM D149
Dissipation Factor 0.0080
@Thickness 3.18 mm,
Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Thickness 3.18 mm
ASTM D696
CTE, linear, Transverse to Flow 63.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 218 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 220 °CHeating rate of 36°F (20°C) per minute.; DSC
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 391 °C
Mold Temperature 138 - 163 °C
Drying Temperature 149 °C
 171 °C
Dry Time 2.50 hour
 4.00 hour
 
Descriptive Properties
Agency RatingsISO 10993
 ISO 10993-Part 1
AppearanceBlue
 Opaque
AvailabilityAsia Pacific
 Europe
 North America
 South America
FeaturesAcid Resistant
 Autoclave Sterilizable
 Base Resistant
 Biocompatible
 E-beam Sterilizable
 Ethylene Oxide Sterilizable
 Flame Retardant
 Good Chemical Resistance
 Good Dimensional Stability
 Good Sterilizability
 Good Thermal Stability
 Good Toughness
 Heat Sterilizable
 High ESCR (Stress Crack Resist.)
 High Heat Resistance
 Hydrolytically Stable
 Radiation (Gamma) Resistant
 Radiation Sterilizable
 Radiotranslucent
 Steam Resistant
 Steam Sterilizable
FormsPellets
GenericPPSU
Processing MethodExtrusion
 Injection Molding
 Machining
 Profile Extrusion
Screw Compression Ratio2.2:1.0
UsesDental Applications
 Hospital Goods
 Medical Appliances
 Medical/Healthcare Applications
 Surgical Instruments

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Radel® RG-5030 Polyphenylsulfone (PPSU)
Syensqo (Solvay Specialty Polymers) Radel® R-7120 Polyphenylsulfone, 20% glass fiber
Syensqo (Solvay Specialty Polymers) Radel® R-5900 Polyphenylsulfone (PPSU)
Syensqo (Solvay Specialty Polymers) Radel® R-5900 MR Polyphenylsulfone (PPSU)
RTP Company RTP 1400 R-5100 Polyphenylsulfone (PPSU)

PSOL8Y7749 / 135808

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.