MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Radel® R-5900 MR Polyphenylsulfone (PPSU)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Radel R-5900 MR polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness. It offers high deflection temperature and outstanding resistance to environmental stress cracking. The resin is inherently flame retardant and has excellent thermal stability and good electrical properties. Radel R-5900 MR is an internally lubricated grade, which offers enhanced mold release. This feature yields the benefits of shorter cycle times and lower injection pressures. Radel R-5900 MR is particularly well suited for applications where design constraints dictate thin walls, tight tolerances and minimal draft angles. - Natural/Transparent: Radel R-5900 NT MR

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Water Absorption 0.37 %
@Time 86400 sec
0.37 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 3.18 mm
0.0070 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 365 °C
30 g/10 min
@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.3 MPa
@Thickness 3.18 mm
10200 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 60 - 120 %
@Thickness 3.18 mm
60 - 120 %
@Thickness 0.125 in
ASTM D638
Elongation at Yield 7.2 %
@Thickness 3.18 mm
7.2 %
@Thickness 0.125 in
ASTM D638
Tensile Modulus 2.34 GPa
@Thickness 3.18 mm
339 ksi
@Thickness 0.125 in
ASTM D638
Flexural Strength 100 MPa
@Thickness 3.18 mm
14500 psi
@Thickness 0.125 in
5.0% Strain; ASTM D790
Flexural Modulus 2.34 GPa
@Thickness 3.18 mm
339 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 6.90 J/cm
@Thickness 3.18 mm
12.9 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
@Thickness 3.18 mm
31.1 µin/in-°F
@Thickness 0.125 in
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
@Thickness 3.18 mm
405 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Glass Transition Temp, Tg 220 °C428 °FASTM E1356
 
Processing PropertiesMetricEnglishComments
Melt Temperature 360 - 391 °C680 - 736 °F
Mold Temperature 138 °C280 °F
Drying Temperature 149 °C300 °F
 171 °C340 °F
Dry Time 4.00 hour4.00 hour
 4.00 hour4.00 hour
 
Descriptive Properties
AdditiveMold Release
AppearanceAmber
 Clear/Transparent
AvailabilityAsia Pacific
 Europe
 North America
 South America
FeaturesAcid Resistant
 Base Resistant
 Flame Retardant
 Good Chemical Resistance
 Good Flow
 Good Mold Release
 Good Thermal Stability
 High ESCR (Stress Crack Resist.)
 High Heat Resistance
 Hydrolytically Stable
 Lubricated
 Steam Sterilizable
 Ultra High Toughness
FormsPellets
GenericPPSU
Processing MethodInjection Molding
Screw Compression Ratio2.2:1.0
UsesAppliances
 Consumer Applications
 Food Service Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Radel® R 5500 Polyphenylsulfone
Syensqo (Solvay Specialty Polymers) Radel® R-5900 Polyphenylsulfone (PPSU)
Syensqo (Solvay Specialty Polymers) Radel® R-7625 Polyphenylsulfone (PPSU)
Syensqo (Solvay Specialty Polymers) Radel® R-7535 Polyphenylsulfone (PPSU)
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)

PSOL8Y7741 / 135800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.