MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Type 254 Fused Quartz Tubing  (discontinued **)
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen and metal halide lamps and other UV sources. Softening point 1615°C. Annealing point 1163°C. Strain point 1066°C.

Data provided by GE Quartz.

GE Quartz became a part of Momentive Performance Materials in 2006.

Key Words: Quartz Tubes
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.21 g/cc
Viscosity 1.30e+14 cP
@Temperature 1100 °C
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 570kg/mm²
Hardness, Mohs 5.5 - 6.5(Type 214)
Modulus of Elasticity 70.0 GPaYoung's Modulus
Compressive Strength 55.0 MPadesign compressive strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 5.00e+10 ohm-cm
@Temperature 350 °C
Dielectric Constant 6.0
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.400 µm/m-°C
@Temperature 20.0 °C
 0.450 µm/m-°C
@Temperature 1000 °C
 0.600 µm/m-°C
@Temperature 500 °C
 0.700 µm/m-°C
@Temperature 250 °C
Specific Heat Capacity 0.690 J/g-°C
@Temperature 0.000 - 50.0 °C
Thermal Conductivity 1.40 W/m-K
Softening Point 1615 °C
Annealing Point 1163 °C
Strain Point 1066 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46
Transmission, Visible 92 %
@Thickness 1.00 mm
(includes surface reflection losses)
IR Transmittance 93 %
@Wavelength 1000 - 3000 nm,
Thickness 1.00 mm
Cutoff is at 5000 nm; (includes surface reflection losses).
UV Transmittance 0.00 %
@Wavelength <=230 nm,
Thickness 1.00 mm
Wavelength dependent - cutoff below 230 nm; less than 5% above 230 nm; (includes surface reflection losses)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Type 214 Fused Quartz Tubing
Quartz (SiO2)
Fused Quartz
Momentive Performance Materials Type 219 Fused Quartz Tubing
96% Silica Consolidated Reconstructed Glass

CGEQ54 / 896

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.