MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Tropical Bubinga Wood
Categories: Wood and Natural Products; Wood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Key Words: Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.710 g/cc0.710 g/ccGreen, African Origin
Density 0.870 g/cc0.0314 lb/inĀ³Air Dry (12-15% Moisture Content)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 12000 N2700 lb (f)Side Hardness, 12% Moisture, African Origin
Tensile Strength, Ultimate 4.10 MPa595 psiPerpendicular to Grain
Modulus of Rupture 0.112 GPa16.2 ksiStatic Bending
 0.1558 GPa22.60 ksiStatic Bending, 12% Moisture, African Origin
Flexural Modulus 12.74 GPa1848 ksiStatic Bending
 17.1 GPa2480 ksiStatic Bending, 12% Moisture, African Origin
Compressive Strength 69.0 MPa10000 psi
 72.4 MPa10500 psiParallel to Grain, 12% Moisture, African Origin
Shear Strength 9.80 MPa1420 psiOrientation Unknown
 21.4 MPa3100 psiParallel to Grain, 12% Moisture, African Origin
Toughness 20.8 J15.3 ft-lb2 cm x 2 cm sample
 
Thermal PropertiesMetricEnglishComments
Shrinkage 5.8 %5.8 %Radial Shrinkage Green to Oven Dry, African Origin
 6.2 %6.2 %Radial; Green to Zero Moisture
 7.7 %7.7 %Tangential; Green to Zero Moisture
 8.4 %8.4 %Tangential Shrinkage Green to Oven Dry, African Origin
 12.7 %12.7 %Volumetric; Green to Zero Moisture
 14.2 %14.2 %Volumetric Shrinkage Green to Oven Dry, African Origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
African Ekki/azobe Wood
AISI 1080 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1080 Steel, cold drawn, spheroidized annealed, 19-32 mm (0.75-1.25 in) round
Sri-Lanka Satinwood Wood
Tropical Aiele Wood

PTST060 / 71388

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.