MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tropical Bubinga Wood
Categories: Wood and Natural Products; Wood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Key Words: Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.710 g/ccGreen, African Origin
Density 0.870 g/ccAir Dry (12-15% Moisture Content)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 12000 NSide Hardness, 12% Moisture, African Origin
Tensile Strength, Ultimate 4.10 MPaPerpendicular to Grain
Modulus of Rupture 0.112 GPaStatic Bending
 0.1558 GPaStatic Bending, 12% Moisture, African Origin
Flexural Modulus 12.74 GPaStatic Bending
 17100 MPaStatic Bending, 12% Moisture, African Origin
Compressive Strength 69.0 MPa
 72.4 MPaParallel to Grain, 12% Moisture, African Origin
Shear Strength 9.80 MPaOrientation Unknown
 21.4 MPaParallel to Grain, 12% Moisture, African Origin
Toughness 20.8 J2 cm x 2 cm sample
 
Thermal PropertiesOriginal ValueComments
Shrinkage 5.8 %Radial Shrinkage Green to Oven Dry, African Origin
 6.2 %Radial; Green to Zero Moisture
 7.7 %Tangential; Green to Zero Moisture
 8.4 %Tangential Shrinkage Green to Oven Dry, African Origin
 12.7 %Volumetric; Green to Zero Moisture
 14.2 %Volumetric Shrinkage Green to Oven Dry, African Origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
African Ekki/azobe Wood
AISI 1080 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1080 Steel, cold drawn, spheroidized annealed, 19-32 mm (0.75-1.25 in) round
Sri-Lanka Satinwood Wood
Tropical Aiele Wood

PTST060 / 71388

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.