MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® LR 8000/10 A/B US Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® LR 8000/10 A/B US is a pourable, two component, addition-curing silicone rubber with short curing time and low hardness.

Special features:

  • fast cure at elevated temperature
  • pourable
  • low hardness
  • very low compression set
Application: Fabrication of soft copy and printer rollers by molding.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³Component A; DIN 53497 A
 1.20 g/cc0.0434 lb/in³Component B
 1.20 g/cc0.0434 lb/in³cured; DIN 53497 A
Viscosity 20000 cP20000 cPComponent B; ISO 3219
 50000 cP50000 cPComponent A; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1010cured; DIN 53505/ISO 868
Tensile Strength at Break 2.10 MPa305 psicured; DIN 53504S1/ISO 37
Elongation at Break 600 %600 %cured; DIN 53504S1/ISO 37
Compression Set 10 %
@Temperature 175 °C,
Time 79200 sec
10 %
@Temperature 347 °F,
Time 22.0 hour
DIN 53517
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
Postcuring 2h/200°C
 
Descriptive Properties
AppearanceBeigeComponent B
 RedComponent A
 Redcured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
NuSil MED-4810 Liquid Silicone Rubber - Unrestricted Medical Use
Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber

PWACK9178 / 204707

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.