MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Performance Alloys MoldStar® 90 Copper Mold Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of thermal conductivity, hardness, corrosion resistance and wear.

Applications:

  • Mold Inserts
  • Thermal Pins
  • Mold Cores
  • Cavities
  • Lifters
  • Etc.

Information provided by Performance Alloys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.58 g/cc0.310 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 3113113000kg
Hardness, Rockwell C 3131
Tensile Strength at Break 1030 MPa150000 psi
Tensile Strength, Yield 965 MPa140000 psi
Elongation at Break 5.0 %5.0 %in 2"
Compressive Strength 965 MPa140000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.1 µm/m-°C
@Temperature 20.0 °C
9.50 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 156 W/m-K
@Temperature 15.6 °C
1080 BTU-in/hr-ft²-°F
@Temperature 60.0 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 89 %89 %
Nickel, Ni 7.5 %7.5 %
Other 3.5 %3.5 %
 
Descriptive Properties
Thermal diffusivity at 68°F1.76 ft²/hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Performance Alloys MoldStar® 150 (PAS 940) Copper Mold Alloy
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, 25.4 - 50.8 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, ≤ 25 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, > 50 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, 25 - 50 mm.

NPER01 / 18768

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.