MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, 25.4 - 50.8 mm.
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: AMPCO 45 is a high strength alloy with mechanical properties beyond the range of commercial nickel-aluminum bronzes. This is due to its special manufacturing process.

Applications: AMPCO 45 is recommended for heavy-duty high-loaded mechanical and corrosive applications. Typical applications involving abrasive wear, friction, deformation, chemical erosion include: aircraft bearings / bushings; pump and marine shafts and wear rings; valve spindles and seats; machine tool parts. The spark-resistance properties make it suitable for safety tools and machine tool components in explosive environments.

Key Words: AMS 4640; ASTM B.150
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.53 g/cc0.272 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217217HB 30
Hardness, Rockwell B 9696
Tensile Strength, Ultimate 793 MPa115000 psi
Tensile Strength, Yield 448 MPa
@Strain 0.5 %
65000 psi
@Strain 0.5 %
Elongation at Break 18 %18 %
Reduction of Area 20 %20 %
Modulus of Elasticity 117 GPa17000 ksi
Compressive Yield Strength 276 MPa40000 psiProportional Limit
Compressive Strength 1000 MPa145000 psi
Fatigue Strength 255 MPa
@# of Cycles 1.00e+8
37000 psi
@# of Cycles 1.00e+8
Shear Strength 476 MPa69000 psi
Izod Impact 13.6 J10.0 ft-lb
Charpy Impact 11.3 J8.33 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000200 ohm-cm0.0000200 ohm-cm9% I.A.C.S.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 °C
9.00 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.450 J/g-°C0.108 BTU/lb-°F
Thermal Conductivity 46.0 W/m-K319 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10 %10 %
Copper, Cu 81 - 81.5 %81 - 81.5 %As Balance
Iron, Fe 2.5 %2.5 %
Manganese, Mn 1.0 %1.0 %
Nickel, Ni 5.0 %5.0 %
Other, total <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C61300, Annealed
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, ≤ 25.4 mm.
Aluminum Bronze D, UNS C61400, Annealed Rod
Aluminum Bronze, UNS C61300, O60 Temper

NAMPCO22 / 14976

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.