MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Overview of materials for Acrylic, Optical Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 - 1.19 g/ccAverage value: 1.18 g/cc Grade Count:23
Water Absorption 0.200 - 0.400 %Average value: 0.300 % Grade Count:12
Thickness 8.00 - 12700 micronsAverage value: 1410 microns Grade Count:9
Linear Mold Shrinkage 0.00200 - 0.00600 cm/cmAverage value: 0.00414 cm/cm Grade Count:7
Melt Flow 5.50 - 21.0 g/10 minAverage value: 12.3 g/10 min Grade Count:3
Spiral Flow 34.0 - 44.0 cmAverage value: 39.3 cm Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 46.0 - 98.0Average value: 85.9 Grade Count:14
Hardness, Rockwell R 106 - 110Average value: 108 Grade Count:5
Tensile Strength, Ultimate 54.0 - 83.0 MPaAverage value: 69.1 MPa Grade Count:8
Tensile Strength, Yield 37.9 - 72.0 MPaAverage value: 55.7 MPa Grade Count:14
Elongation at Break 4.00 - 5.80 %Average value: 4.91 % Grade Count:12
Elongation at Yield 3.90 - 6.60 %Average value: 5.43 % Grade Count:3
Modulus of Elasticity 1.52 - 3.38 GPaAverage value: 2.62 GPa Grade Count:25
Flexural Yield Strength 57.0 - 120 MPaAverage value: 101 MPa Grade Count:20
Flexural Modulus 1.86 - 3.38 GPaAverage value: 2.83 GPa Grade Count:16
Compressive Yield Strength 117 - 124 MPaAverage value: 119 MPa Grade Count:3
Izod Impact, Notched 0.149 - 1.10 J/cmAverage value: 0.425 J/cm Grade Count:7
 0.200 - 0.500 J/cm
@Temperature -18.0 - -18.0 °C
Average value: 0.275 J/cm Grade Count:4
Izod Impact, Unnotched 0.320 - 0.587 J/cmAverage value: 0.427 J/cm Grade Count:5
Izod Impact, Notched (ISO) 0.400 - 0.750 kJ/m²Average value: 0.603 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.37 - 5.00 J/cm²Average value: 2.02 J/cm² Grade Count:8
Charpy Impact, Notched 0.120 - 0.130 J/cm²Average value: 0.123 J/cm² Grade Count:3
Gardner Impact 0.226 - 5.30 JAverage value: 2.42 J Grade Count:7
Falling Dart Impact 8.13 - 13.6 JAverage value: 10.3 J Grade Count:5
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 40.0 - 120 dBAverage value: 73.8 dB Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 52.2 - 162 µm/m-°CAverage value: 104 µm/m-°C Grade Count:28
Thermal Conductivity 0.0252 - 0.190 W/m-KAverage value: 0.0892 W/m-K Grade Count:10
Maximum Service Temperature, Air 60.0 - 100 °CAverage value: 75.6 °C Grade Count:22
Deflection Temperature at 0.46 MPa (66 psi) 96.0 - 101 °CAverage value: 98.1 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 71.0 - 99.0 °CAverage value: 88.9 °C Grade Count:20
Vicat Softening Point 99.0 - 116 °CAverage value: 106 °C Grade Count:13
Minimum Service Temperature, Air -55.0 - -34.0 °CAverage value: -51.5 °C Grade Count:4
Flammability, UL94 HBGrade Count:5
Flame Spread 15.2 - 25.9 mm/minAverage value: 20.5 mm/min Grade Count:3
Smoke Density 0.0200 - 20.0Average value: 3.68 Grade Count:10
Ignition Temperature 399 - 488 °CAverage value: 446 °C Grade Count:11
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46 - 1.49Average value: 1.49 Grade Count:14
Haze 1.00 - 3.00 %Average value: 1.78 % Grade Count:7
Gloss 90.0 - 140 %Average value: 104 % Grade Count:6
Transmission, Visible 28.0 - 92.0 %Average value: 78.4 % Grade Count:24
UV Transmittance 92.0 %Average value: 92.0 % Grade Count:3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 143 - 160 °CAverage value: 156 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Optical Grade, Molded
Trinseo Plexiglas® Diffuse™ V045-68207 Acrylic Resin
Trinseo Plexiglas® VS-UVT Acrylic
Trinseo Solarkote™ A200 Acrylic
Overview of materials for Acrylic, General Purpose, Molded

O1336 / 77870

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.