MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Escorene™ Ultra LD 730.PM Ethylene Vinyl Acetate Copolymer (EVA)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Escorene Ultra LD 730 series are 17.2% wt vinyl acetate copolymer resins.  These resins are designed to have superior strength and toughness combined with excellent optics and sealing properties..  

Availability: North America, Latin America.  Additives: antiblock: no; slip: no; thermal stabilizer: yes. 

Applications:  heat seal layer, pallet shrink film, stretch film.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D1505
Vinyl Acetate Content 17.2 %17.2 %ExxonMobil Method
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 360 %360 %ASTM D882
Film Elongation at Break, TD 660 %660 %ASTM D882
Puncture Energy 6.10 J4.50 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 50 g50 gASTM D1922
Elmendorf Tear Strength TD 120 g120 gASTM D1922
Dart Drop Test 670 g1.48 lbASTM D1709A
Film Tensile Strength at Break, MD 37.2 MPa5400 psiASTM D882
Film Tensile Strength at Break, TD 37.9 MPa5500 psiASTM D882
1% Secant Modulus, MD 57.2 MPa8300 psiASTM D882
1% Secant Modulus, TD 64.1 MPa9300 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 87.8 °C190 °FPeak; ExxonMobil Method
Vicat Softening Point 65.0 °C149 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 1.5 %1.5 %ASTM D1003
Gloss 86 %86 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98929 / 238310

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.