Escorene Ultra LD 730 series are 17.2% wt vinyl acetate copolymer resins. These resins are designed to have superior strength and toughness combined with excellent optics and sealing properties.. Availability: North America, Latin America. Additives: antiblock: no; slip: no; thermal stabilizer: yes. Applications: heat seal layer, pallet shrink film, stretch film. Information provided by ExxonMobil. |