System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® ECO PA GF30 909040 Nylon 6, 30% Glass Fiber
Categories:
Polymer
;
Renewable/Recycled Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 30% Glass Fiber Filled
Material Notes:
PA 6 (mainly), 30% glass fibers, injection molding, contains at least 80% pre-consumer recycled material, properties may change considerably from lot to lot
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.36
g/cc
ISO 1183
Moisture Absorption at Equilibrium
2.1 %
50% RH; ISO 62
Water Absorption at Saturation
7.0 %
ISO 62
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
135
MPa
d.a.m.; ISO 527-1, -2; 5 mm/min
Elongation at Break
2.5 %
d.a.m.; ISO 527-1, -2; 5 mm/min
Tensile Modulus
8500
MPa
d.a.m.; ISO 527-1, -2; 1 mm/min
Flexural Strength
210
MPa
@Strain 3 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Modulus
7500
MPa
d.a.m., 2 mm/min; ISO 178-A
Izod Impact, Unnotched (ISO)
40.0
kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 180-1U
Charpy Impact Unnotched
50.0
kJ/m²
d.a.m.; ISO 179-1eU
Thermal Properties
Original Value
Comments
Melting Point
>=
210
°C
10°C/min; ISO 11357-1, -3
Processing Properties
Original Value
Comments
Melt Temperature
270
-
290
°C
280
°C
for test specimens; ISO 294
Mold Temperature
80.0
°C
for test specimens; ISO 294
80.0
-
120
°C
Drying Temperature
80.0
°C
Dry Time
2
-
6
hour
Moisture Content
0.030 - 0.12 %
residual; Karl Fischer Test
Descriptive Properties
ISO Short Name
ISO 1874-PA 6/XX, GR, 14-080, GF30
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 1 L black (4652) PA 66 + PP Dry
EMS-Grivory Grivory® GV-2 FWA nat PA*-GF20
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 15 pcf
ExxonMobil Mobil ATF D/M
PLANX0651 / 133614
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.