MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 15 pcf
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Baydur 645 is a rigid polyurethane structural foam system used in the reaction injection molding (RIM) process.

Properties / Applications: Baydur 645 is a rigid polyurethane structural foam system used in the reaction injection molding (RIM) process. The system is supplied as two reactive liquid components. Component A is a polymeric diphenylmethane diisocyanate (PMDI), and Component B is a formulated polyol system containing no CFC- or HCFC-blowing additives. The Baydur 645 system is used to produce foam cores for composite applications, such as water skis, agricultural and construction equipment, and various components for the transportation and marine markets. As with any product, use of the Baydur 645 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity  0.240 g/cc
@Thickness 6.35 mm
0.240 g/cc
@Thickness 0.250 in
ASTM D792
 0.240 g/cc
@Thickness 12.7 mm
0.240 g/cc
@Thickness 0.500 in
ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  28
@Thickness 6.35 mm
28
@Thickness 0.250 in
ASTM D2240
 30
@Thickness 12.7 mm
30
@Thickness 0.500 in
ASTM D2240
Tensile Strength at Break  3.79 MPa
@Thickness 12.7 mm
550 psi
@Thickness 0.500 in
ASTM D638
 3.86 MPa
@Thickness 6.35 mm
560 psi
@Thickness 0.250 in
ASTM D638
Elongation at Break  7.0 %
@Thickness 6.35 mm
7.0 %
@Thickness 0.250 in
ASTM D638
 9.0 %
@Thickness 12.7 mm
9.0 %
@Thickness 0.500 in
ASTM D638
Flexural Strength  6.55 MPa
@Thickness 6.35 mm
950 psi
@Thickness 0.250 in
ASTM D790
 6.89 MPa
@Thickness 12.7 mm
999 psi
@Thickness 0.500 in
ASTM D790
Flexural Modulus  0.186 GPa
@Thickness 12.7 mm
27.0 ksi
@Thickness 0.500 in
ASTM D790
 0.221 GPa
@Thickness 6.35 mm
32.1 ksi
@Thickness 0.250 in
ASTM D790
Compressive Strength  1.90 MPa
@Thickness 12.7 mm
276 psi
@Thickness 0.500 in
ASTM D695
 2.96 MPa
@Thickness 6.35 mm
429 psi
@Thickness 0.250 in
ASTM D695
Charpy Impact Unnotched  0.378 J/cm²
@Thickness 6.35 mm
1.80 ft-lb/in²
@Thickness 0.250 in
 0.399 J/cm²
@Thickness 12.7 mm
1.90 ft-lb/in²
@Thickness 0.500 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Covestro Bayfill® EA 2001 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System
Elliott Company ELFOAM® P200 Polyisocyanurate Foam
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,

PCOVEST0082 / 201865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.