Titanvene™ LL0335AA is a linear low density polyethylene designed for silane crosslinked low voltage power cable insulation, casting film and inner layer for rotomolding. Titanvene™ LL0335AA characterized by high speed performance, low gel content and easy extrusion Applications: Low voltage power cable insulation for sioplas process; Casting film; Inner layer for rotomolding (Non UV) Information provided by Lotte Advanced Materials. |