MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Titanvene™ LL0335AA LLDPE Film
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Titanvene™ LL0335AA is a linear low density polyethylene designed for silane crosslinked low voltage power cable insulation, casting film and inner layer for rotomolding. Titanvene™ LL0335AA characterized by high speed performance, low gel content and easy extrusion

Applications: Low voltage power cable insulation for sioplas process; Casting film; Inner layer for rotomolding (Non UV)

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/ccISO 1183 Method D
Melt Flow 3.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133 Condition 4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 143 kg(f)/cm²Type 2 Speed C; ISO/R 527
Elongation at Break 1400 %Type 2 Speed C; ISO/R 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.54ASTM D150
Dissipation Factor <= 0.000100ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 121 °CISO 3146 Method C
Vicat Softening Point 105 °CISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOTT9611 / 326093

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.