MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
KiON CERASET® ULTRA POLYSILIZANE Melt-Fusible Ceramic Precursor  (discontinued **)
Categories: Polymer; Thermoset

Material Notes: KiON CERASET Ultra is a solid polysilazane that softens upon heating. KiON CERASET Ultra Polysilazane can be melt- or solvent- spun into fibers. Fibers spun from KiON Ceraset Ultra Polysilazane are readily shape stabilized prior to pyrolysis by various methods including radical- or UV-initiated curing processes. The resulting fibers can then be pyrolyzed to silicon carbide, silicon nitride, silicon carbonitride, or silicon carboxynitride by heating to 1,000°C. The final ceramic phase is dependent upon the pyrolysis atmosphere. The ceramic yield as measured by thermal gravimetric analysis (TGA) is 84 % in a nitrogen atmosphere.

Applications

Ceramic Fibers, Ceramic Matrix Composites (CMC’s), Metal Matrix Composites (MMC’s), Ceramic Joining, SiC/Si3N4 coatings for C/C composites.

Information provided by KiON Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/cc
 2.40 g/ccCeramic from Pyrolysis
 
Descriptive Properties
AppearanceWhite to pale yellow solid

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ferro Silicon Nitride
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4)
Ceradyne Ceralloy® 147-5 Silicon Nitride
Ceradyne Ceralloy® 147-31N Silicon Nitride

PKION01 / 48717

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.