MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ceradyne Ceralloy® 147-5 Silicon Nitride  (discontinued **)
Categories: Ceramic; Nitride

Material Notes: Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's silicon nitrides. Finished components are machined at Ceradynes precision diamond grinding facility.

Applications: wear components.

Information provided by Ceradyne Company

Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.30 g/cc0.119 lb/in³
Weibull Modulus 15 - 2015 - 20
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 180018000.3 kg/mm²
Modulus of Elasticity 320 GPa46400 ksi
Flexural Strength 930 MPa
@Temperature 23.0 °C
135000 psi
@Temperature 73.4 °F
Poissons Ratio 0.280.28
Fracture Toughness 6.00 MPa-m½5.46 ksi-in½
Shear Modulus 125 GPa18100 ksicalculated
Abrasion 11001100Abrasive Wear Resistance Parameter
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Constant 8.148.14
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.20 µm/m-°C
@Temperature 20.0 - 1000 °C
1.78 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 35.0 W/m-K243 BTU-in/hr-ft²-°F
 
Descriptive Properties
Purity, %>98.5
Thermal Shock Parameter654°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Techical Ceramics Ekasic® S Silicon Nitride
Ceradyne Ceralloy® 147-1E Silicon Nitride
Silicon Nitride
3M Techical Ceramics Ekatherm® Silicon Nitride
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3

CCERDN03 / 686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.