Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inch thick sheets. These test pieces were exposed for 120 hours to a cycle consisting of: 1. Light at 70°C for 8 hours 2. Dark at 50° C for 4 hours 3. Condensation Cooling for 15 minutesInformation provided by Monmouth Rubber & Plastics Corp. |